things might have actually been warping a bit more with the higher temps

at least it's seeming that way with some Bambu matte PLA

Signed-off-by: Brian S. Stephan <bss@incorporeal.org>
This commit is contained in:
Brian S. Stephan 2024-04-01 16:11:43 -05:00
parent b21cb75816
commit 45439cbf6d
Signed by: bss
GPG Key ID: 3DE06D3180895FCB

View File

@ -32,8 +32,6 @@ plates, etc. will cover it up. However, I've had some interesting results with:
* Initial layer line width: 0.42mm (down .08mm) * Initial layer line width: 0.42mm (down .08mm)
* Initial layer height: 0.25mm (up .05mm) * Initial layer height: 0.25mm (up .05mm)
* Initial layer nozzle temperature: 230°C (up 10°C)
* Initial layer bed temperature: 70°C (up 5°C)
* Initial layer pattern: concentric * Initial layer pattern: concentric
These are good defaults and print awesome parts, with the only exception being the top panels, which benefit from using These are good defaults and print awesome parts, with the only exception being the top panels, which benefit from using